Michael Wang

Founder & Mechanical Engineer

As the founder of the company and a mechanical engineer, he has extensive experience in advanced manufacturing technologies, including CNC machining, 3D printing, urethane casting, rapid tooling, injection molding, metal casting, sheet metal, and extrusion.

Table Of Contents

Explore CNC Design & Material Selection

Delrin is the material engineers reach for when a plastic part has to hold a tolerance and slide against something. It machines cleanly, holds its size far better than nylon, and fails in one specific way that is worth designing around.

Can Delrin be machined?

Yes, and it is one of the easiest plastics to machine well.

Delrin, the trade name for POM or acetal, is a semi-crystalline thermoplastic with high stiffness, low friction and very low moisture absorption. It produces clean chips rather than the stringy swarf that polyolefins generate, holds a good surface finish from a sharp tool, and does not swell with humidity the way nylon does. That combination makes it the default choice for precision mechanical parts at low volume.

The material also machines predictably at high speeds. Because it is stiff, it deflects less under cutting load than a soft polyolefin, so dimensions are easier to hold and finishing passes behave as expected. The main precautions are the usual ones for plastics: sharp tooling, adequate chip clearance and a rigid setup to avoid vibration marking the surface.

Are POM and Delrin the same thing?

Yes, Delrin is a brand name for POM.

Delrin is a brand name for polyoxymethylene, usually abbreviated POM, so the two words describe the same polymer family. As with other trade names, the practical issue is specification: a drawing that calls only for “Delrin” leaves the supplier to infer a grade, and POM is supplied in homopolymer and copolymer forms that differ in stiffness, chemical resistance and machining behaviour. Naming the material and the grade removes that ambiguity.

Two distinctions matter in practice. Homopolymer POM is generally stiffer and harder, while copolymer POM offers better chemical resistance and thermal stability. And filled grades exist, with glass or PTFE additions, which improve stiffness or reduce friction at the cost of machinability and surface finish. Material property data is published by ASM International.

Property What it means in a machined part
Moisture absorption Very low, so dimensions stay stable in humid conditions
Friction and wear Low friction; suits bearings, bushings and sliding parts
Stiffness High for a plastic, so thin sections hold shape better
Chemical resistance Good against many solvents, poor against strong acids
Bonding and painting Difficult without surface treatment
Notch behaviour Sensitive; sharp corners crack under load
Machined engineering plastic component produced to close tolerance from POM stock
Acetal machines cleanly and holds size: the difficulty is design, not the cut.

What are the disadvantages of Delrin?

Notch sensitivity, poor bonding, limited heat range.

Four limitations recur. The material is notch sensitive, so a sharp internal corner or a sudden section change becomes a crack origin under load or impact. It is difficult to bond or paint, because its low surface energy resists adhesion, so joints usually need mechanical fastening. It has a limited temperature range compared with engineering plastics such as PEEK or PEI, softening well below them. And it is attacked by strong acids and some oxidising chemicals, which rules it out for aggressive media despite good general chemical resistance.

A fifth characteristic deserves attention because it causes real failures: POM can be degraded by contact with certain chemicals in service, and it is also sensitive to chlorine-containing water in some conditions. Where a part will meet a specific medium, checking the compatibility of the grade against that medium is more reliable than assuming general chemical resistance applies.

Does Delrin crack easily?

Cracks start at notches, tight fits or chemicals.

Cracks in POM almost always start from one of three causes. A sharp internal corner or a machined scratch acts as a stress raiser, and under load or repeated cycling a crack begins there. A part assembled under interference can be over-stressed, particularly if the fit was calculated for a metal and applied to plastic. And chemical attack can embrittle the material, after which even modest stress produces cracking.

The design responses are consistent. Radius internal corners generously, avoid sharp shoulders, and specify a machined finish that does not leave deep tool marks in a stressed area. Design interference fits with plastic behaviour in mind rather than copying a metal fit, and check chemical compatibility before committing to the material. Where a part must survive both load and chemical exposure, a different polymer is often the better answer.

Where machined POM is the right choice

Four applications dominate. Precision mechanical components such as gears, cams and bushings, where dimensional stability and low friction matter. Parts that slide, including guides, wear pads and rollers, since POM runs well against steel and against itself. Fluid-handling components, where its low moisture absorption and chemical resistance suit fittings and valve parts. And fixtures and jigs, where stiffness and machinability make it a practical alternative to metal.

It is the wrong choice where the part will see high continuous temperature, strong acids, or a structural load that requires a metal. It is also the wrong choice where the part must be bonded rather than fastened, because adhesive performance on POM is poor without treatment. Where the requirement is a wear surface at higher temperature, PEEK is often the material that replaces it. Machining and molding routes are described under CNC machining and injection molding.

Specifying a POM part

Name the polymer and the grade, including homopolymer or copolymer and any filler, since these change stiffness, friction and machining behaviour. State the chemicals and the temperature range the part will encounter, identify the sliding or loaded surfaces, and specify the internal radii at any transition where stress will concentrate. Where the part is a bearing or a bushing, state the mating material and the shaft fit, because wear depends on the pair rather than on POM alone.

Two details improve the outcome. State the measurement condition and the stabilisation period, because even a low-absorption material changes slightly after machining as it cools. And avoid specifying a tight tolerance on a non-functional surface, since the effort is better spent on the fits that determine whether the part works. Drawing conventions follow ASME standards, surface terminology follows ASTM Committee B08, measurement practice is described by the NIST Manufacturing Extension Partnership, and process obligations are set out by the US EPA. Comparative material behaviour is set out under materials.

Machined black plastic components where radii prevent cracking in a notch sensitive material
Radius the shoulders: in a notch-sensitive plastic, the crack starts at the sharpest point.

Send the part with the fit, the mating material and the chemicals involved, and request a POM machining quote with the grade specified.

FAQ

Can Delrin be machined?

Yes, and it is one of the easiest plastics to machine well. It produces clean chips, holds a good surface finish and has very low moisture absorption, so it maintains dimensions far better than nylon. Sharp tooling and a rigid setup are the main requirements.

Are POM and Delrin the same thing?

Delrin is a brand name for POM, polyoxymethylene, so the two describe the same polymer family. Grades differ between homopolymer and copolymer, and fillers change stiffness and friction, so a drawing should name the grade rather than the brand.

What are the disadvantages of Delrin?

Notch sensitivity that makes sharp corners crack origins, difficulty bonding or painting without surface treatment, a temperature range below high-performance plastics such as PEEK, and vulnerability to strong acids and some oxidising chemicals.